Service hotline: 86-769-82884411
¡¡Manufacturing process
¡¡Direction fo use
¡¡Note
 
1. Use standard mixing ratio - Water(ml) : Powder(100g).
2. Add water first, then slowly adding powder into the water.
3. Mixing time: 30~60 Sec.
4. Remove from the impression: 30 Min. after the stone is poured.
5. Using vibrator could be get smooth and bubble-free surface of model.